Sign In | Join Free | My bushorchimp.com
China Beijing Tonghe Testing Machine Co., ltd logo
Beijing Tonghe Testing Machine Co., ltd
WE OFFER ONLY WHAT SUITS YOU BEST!
Verified Supplier

2 Years

Home > Differential Scanning Calorimeter >

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement

Beijing Tonghe Testing Machine Co., ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement

  • 1
  • 2

Brand Name : TH

Model Number : DSC-ZS5

Certification : ISO9001 CE

Place of Origin : BEIJING, CHINA

MOQ : 1 set

Payment Terms : L/C,D/A,D/P,T/T,Western Union,MoneyGram

Supply Ability : 20 sets per month

Delivery Time : 10~15 work days

Packaging Details : Standard export wooden box

Product name : Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement

Temperature resolution : 0.01 ℃

Heating rate : 0.1~40℃/min

Cooling rate : 0.1~20℃/min

DSC range : 0 ~ + 500 mw

DSC resolution : 0.01 mW

DSC sensitivity : 0.01 mW

Temperature control mode : Heating, cooling, constant temperature

Contact Now

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement



Summary:

This DSC (Differential Scanning Calorimeter) features a touchscreen interface, specifically engineered for the oxidation induction period (OIT) testing of polymeric materials. It supports one-key operation for users and full software automation—streamlining testing workflows and ensuring consistent, error-free operation.

The instrument fully complies with the following international and national standards:

  • GB/T 19466.2-2009 / ISO 11357-2:1999
  • GB/T 19466.3-2009 / ISO 11357-3:1999
  • GB/T 19466.6-2009 / ISO 11357-6:1999


Features:

  • Industrial-Grade Widescreen Touch Interface

    Boasts an information-rich display presenting comprehensive real-time data, including set temperature, sample temperature, oxygen flow rate, nitrogen flow rate, differential thermal signal, and various switch statuses—facilitating intuitive monitoring and operation.
  • Universal USB Communication Interface

    Features high universality and reliable data transmission, with built-in self-recovering connection functionality. This ensures stable communication with external devices and minimizes interruptions during testing.
  • Compact Furnace with Adjustable Thermal Rates

    Adopts a compact furnace structure, supporting stepless adjustment of heating and cooling rates to meet the thermal cycle requirements of different polymeric material OIT tests.
  • Optimized Installation & Anti-Contamination Design

    Equipped with an improved installation process and adopts a mechanical fastening method. This completely eliminates contamination of the differential thermal signal caused by internal furnace colloid, ensuring the accuracy of test data.
  • Efficient Heating & Cooling System

    The furnace utilizes electric heating wires for heating and circulating cooling water (compressor-refrigerated) for cooling. It features a compact structure and small footprint, saving laboratory space while ensuring efficient thermal regulation.
  • High-Precision Temperature Control

    Dual temperature probes guarantee excellent repeatability of sample temperature measurement. Specialized temperature control technology is employed to regulate the furnace wall temperature, thereby achieving precise control of the sample’s set temperature.
  • Automatic Gas Channel Switching

    The gas flow meter enables automatic switching between two gas channels, with fast switching speed and short stabilization time—ensuring consistent gas atmosphere conditions during testing.
  • Standard Reference Samples for Calibration

    Comes with standard reference samples, facilitating convenient calibration of temperature coefficients and enthalpy coefficients to maintain long-term testing accuracy.
  • Versatile Software Compatibility

    The software supports screens of all resolutions, automatically adjusting the computer screen size and curve display mode. It is fully compatible with laptops and desktops, and supports multiple operating systems including Windows 2000, XP, Vista, Windows 7, Windows 8, and Windows 10.
  • Customizable Automated Operation

    Supports users in editing device operation modes based on actual testing requirements, realizing full automation of measurement steps. The software provides dozens of configurable instructions, allowing users to flexibly combine and save instructions according to specific test procedures—simplifying complex operations into one-click execution.
  • Fully Enclosed Protective Structure

    Adopts a fully enclosed support structure design, which prevents foreign objects from falling into the furnace body, avoids furnace contamination, and reduces maintenance frequency.

Parameters:

Temperature range 0℃~500℃
Temperature resolution 0.01℃
Heating rate 0.1~40℃/min
Cooling rate 0.1~20℃/min
Calorimetric resolution 100%.
Constant temperature 5℃~500℃
Duration of constant temperature The duration is recommended to be less than 24 hours.
Temperature control mode Heating, cooling, constant temperature
DSC range 0~±500mW
DSC resolution 0.01mW
DSC sensitivity 0.01mW
Working power AC 220V 50Hz 300W or other
Atmosphere control gas Two-channel gas control by automatic controlled (e.g. nitrogen and oxygen)
Gas flow 0-200mL/min
Gas pressure 0.2MPa
Gas flow accuracy 0.2mL/min
Crucible Aluminium crucible Φ6.6*3mm (Diameter * High)
Calibration standard with standard material (indium, tin, zinc)
Data interface Standard USB interface
Display mode 7-inch touch screen
Output mode computer and printer


Configuration list:

DSC machine 1 set
Aluminium crucibles 300 pieces
Power cords and USB cable Each one
CD (contains software and operations video) One
Soft-key One
Oxygen airway and nitrogen airway Each 5m
Operation manual One
Standard sample(contains Indium, tin, zinc) Each one
Tweezer and medicine spoon Each one
Custom pressure reducing valve joint and quick joint Two
Fused glass fuses Four
External circulation thermostat sink One
Water pipe One


Furnace bracket:

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement


Software screenshots:

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement


Product Tags:

Industrial differential scanning calorimeter with touch interface

      

Polymer oxidation induction period calorimeter

      

Widescreen DSC for accurate measurements

      
Buy cheap Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement product

Industrial Differential Scanning Calorimeter Featuring Widescreen Touch Interface for Accurate Polymer Oxidation Induction Period Measurement Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Beijing Tonghe Testing Machine Co., ltd
*Subject:
*Message:
Characters Remaining: (0/3000)